Physical Properties Metric English Comments
Viscosity 281800 cP

@Shear Rate 500 1/s,
Temperature 200 °C
281800 cP

@Shear Rate 500 1/s,
Temperature 392 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..