Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3.8 cP @Temperature 79.4 °C |
3.8 cP @Temperature 175 °F |
|
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and.. |
|||
Viscosity | 3.8 cP @Temperature 45.0 °C |
3.8 cP @Temperature 113 °F |
|
LG Chemical Phenol Structure & Characteristics: C6H5OH. Phenol is a white crystalline solid with a distinct smellUses: Raw material of phenolic resins, dye stuffs, synthetic fibers, herbicides, photo material, aromati.. |