Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 40000 cP @Shear Rate 1340 1/s, Temperature 200 °C |
40000 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Viscosity | 40000 cP @Shear Rate 1340 1/s, Temperature 200 °C |
40000 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynalloy™ OBC8000-T05 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T05 is an ultra-soft TPE utilizing the unique rubber properties of Dows INFUSE™ Olefin Block Copolymers. This product is designed for injection molding applications where excepti.. |
|||
Viscosity | 40000 - 50000 cP @Temperature 25.0 °C |
40000 - 50000 cP @Temperature 77.0 °F |
TA4202A |
Permabond TA4202 Toughened Acrylic Adhesive PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Viscosity | 40000 - 50000 cP @Temperature 25.0 °C |
40000 - 50000 cP @Temperature 77.0 °F |
TA4202B |
Permabond TA4202 Toughened Acrylic Adhesive PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Viscosity | 40000 - 60000 cP @Temperature 25.0 °C |
40000 - 60000 cP @Temperature 77.0 °F |
TA4592A, at 2.5 rpm vibration |
Permabond TA4592 Toughened Acrylic Adhesive PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt.. |
|||
Viscosity | 40000 - 60000 cP @Temperature 25.0 °C |
40000 - 60000 cP @Temperature 77.0 °F |
TA4592A |
Permabond TA4810 Toughened Acrylic Adhesive PERMABOND TA4810 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4810 has excellent adhesion to as received metal surfac.. |
|||
Viscosity | 40000 - 60000 cP @Temperature 25.0 °C |
40000 - 60000 cP @Temperature 77.0 °F |
TA4592B |
Permabond TA4810 Toughened Acrylic Adhesive PERMABOND TA4810 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4810 has excellent adhesion to as received metal surfac.. |
|||
Viscosity | 40000 - 60000 cP @Temperature 25.0 °C |
40000 - 60000 cP @Temperature 77.0 °F |
TA4820A |
Permabond TA4820 Structural Acrylic Adhesive PERMABOND TA4820 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4820 has excellent adhesion to as received metal surfac.. |
|||
Viscosity | 40000 - 60000 cP @Temperature 25.0 °C |
40000 - 60000 cP @Temperature 77.0 °F |
TA4820B |
Permabond TA4820 Structural Acrylic Adhesive PERMABOND TA4820 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4820 has excellent adhesion to as received metal surfac.. |
|||
Viscosity | 40000 cP @Temperature 25.0 °C |
40000 cP @Temperature 77.0 °F |
Resin |
Lord Adhesives Thermosetâ„¢ EP-809 Ignition Coil Impregnating and Encapsulation Epoxy Lord EP-809 is a long working life, heat curing, two component epoxy formulation. It was designed especially for potting high voltage automotive ignition coils. The combination of low viscosity, exc.. |
|||
Viscosity | 40000 cP @Shear Rate 5000 1/s, Temperature 190 °C |
40000 cP @Shear Rate 5000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ IP-50 High Density Polyethylene DOWLEX® IP-50 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution designed for thin wall food containers. This resin is recommended for flo.. |
|||
Viscosity | 40000 cP @Shear Rate 5000 1/s, Temperature 190 °C |
40000 cP @Shear Rate 5000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow LDPE 779I Low Density Polyethylene DOW LDPE 779I resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent rigidity. Typical applications include caps.. |
|||
Viscosity | 40000 cP @Shear Rate 300 1/s, Temperature 190 °C |
40000 cP @Shear Rate 300 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow LDPE 959I Low Density Polyethylene DOW LDPE 959I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility with low warpage for lids. This resin has good processability over a wi.. |
|||
Viscosity | 40000 cP @Shear Rate 5000 1/s, Temperature 315 °C |
40000 cP @Shear Rate 5000 1/s, Temperature 599 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Viscosity | 40000 cP @Frequency 1000 Hz, Temperature 307 °C |
40000 cP @Frequency 1000 Hz, Temperature 585 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Viscosity | 40000 cP @Temperature 25.0 °C |
40000 cP @Temperature 77.0 °F |
at 2 rpm vibration |
Permabond A131 Anaerobic Threadsealant Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an.. |