Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4400 cP @Temperature 25.0 °C |
4400 cP @Temperature 77.0 °F |
Mixed; STM 1 |
Lord Adhesives Thermosetâ„¢ UR-329 Two Component Urethane Potting Compound Lord UR-329 is a flexible, two-component, room temperature curing, urethane, encapsulating compound. UR-329 maintains low hardness and modulus over a wide temperature range, which imparts minimal st.. |