Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 509000 cP @Shear Rate 500 1/s, Temperature 215 °C |
509000 cP @Shear Rate 500 1/s, Temperature 419 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AF is a high viscosity acetal homopolymer containing 20% Teflon PTFE fibers. It is designed for a.. |