Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 60000 - 650000 cP @Temperature 400 - 400 °C |
60000 - 650000 cP @Temperature 752 - 752 °F |
Average value: 396000 cP Grade Count:5 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Viscosity | 60000 - 650000 cP @Shear Rate 1000 - 1000 1/s |
60000 - 650000 cP @Shear Rate 1000 - 1000 1/s |
Average value: 396000 cP Grade Count:5 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Viscosity | 60000 cP @Shear Rate 5000 1/s, Temperature 290 °C |
60000 cP @Shear Rate 5000 1/s, Temperature 554 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough.. |
|||
Viscosity | 60000 cP @Shear Rate 1000 1/s, Temperature 190 °C |
60000 cP @Shear Rate 1000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2500 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with high impact strength. It.. |
|||
Viscosity | 60000 cP @Shear Rate 300 1/s, Temperature 190 °C |
60000 cP @Shear Rate 300 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow LDPE 955I Low Density Polyethylene DOW LDPE 955I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility, and good toughness, with low warpage. Typical applications include lid.. |
|||
Viscosity | 60000 - 70000 cP @Temperature 25.0 °C |
60000 - 70000 cP @Temperature 77.0 °F |
ET514A, Epoxy Resin |
Permabond ET514 Epoxy Resin PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu.. |