Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 60000 - 70000 cP @Temperature 25.0 °C |
60000 - 70000 cP @Temperature 77.0 °F |
ET514A, Epoxy Resin |
Permabond ET514 Epoxy Resin PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu.. |