Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 65000 cP @Shear Rate 5000 1/s, Temperature 230 °C |
65000 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Viscosity | 65000 cP @Temperature 25.0 °C |
65000 cP @Temperature 77.0 °F |
at 2 rpm vibration |
Permabond MH052 Anaerobic Threadsealant Permabond® MH052 is ideal for the sealing of threaded joints. It is approved for use with natural gas and LPG for working pressure up to 20 bar (290 psi) and also for gaseous oxygen up to 10 bar (1.. |