Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 700000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 700000 cP

@Shear Rate 1.00 1/s,
Temperature 250 °C
700000 cP

@Shear Rate 1.00 1/s,
Temperature 482 °F
DSM Arnite® TV4 441 (PBT+PET)-GF20
20% Glass Reinforced
Viscosity 700000 cP

@Shear Rate 1.00 1/s,
Temperature 230 °C
700000 cP

@Shear Rate 1.00 1/s,
Temperature 446 °F
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40
20% Glass Reinforced, 20% Glass Beads Reinforced
Viscosity 700000 cP

@Shear Rate 0.100 1/s,
Temperature 280 °C
700000 cP

@Shear Rate 0.100 1/s,
Temperature 536 °F
DSM Novamid® 2320J PA666
Extrusion
Viscosity 700000 cP

@Shear Rate 1.00 1/s,
Temperature 230 °C
700000 cP

@Shear Rate 1.00 1/s,
Temperature 446 °F
DSM Arnite® TZ6 280 PBT-(GF+GB)40
20% Glass Reinforced, 20% Glass Beads Reinforced
Copyright © lookpolymers.com All Rights Reserved