Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Arnite® TV4 441 (PBT+PET)-GF20

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled
Manufacturer DSM Engineering Plastics
Trade Name Arnite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® TV4 441 (PBT+PET)-GF20.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Glass Reinforced
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Water Absorption 0.30 %
0.30 %
Sim. To ISO 62
Moisture Absorption 0.150 %
0.150 %
Sim. To ISO 62
Viscosity 12500 cP

@Shear Rate 100000 1/s,
Temperature 270 °C
12500 cP

@Shear Rate 100000 1/s,
Temperature 518 °F
17500 cP

@Shear Rate 100000 1/s,
Temperature 250 °C
17500 cP

@Shear Rate 100000 1/s,
Temperature 482 °F
20000 cP

@Shear Rate 100000 1/s,
Temperature 230 °C
20000 cP

@Shear Rate 100000 1/s,
Temperature 446 °F
300000 cP

@Shear Rate 1.00 1/s,
Temperature 270 °C
300000 cP

@Shear Rate 1.00 1/s,
Temperature 518 °F
700000 cP

@Shear Rate 1.00 1/s,
Temperature 250 °C
700000 cP

@Shear Rate 1.00 1/s,
Temperature 482 °F
1.00e+6 cP

@Shear Rate 1.00 1/s,
Temperature 230 °C
1.00e+6 cP

@Shear Rate 1.00 1/s,
Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 112 MPa
16200 psi
ISO 527-1/-2
Elongation at Break 2.7 %
2.7 %
ISO 527-1/-2
Tensile Modulus 7.30 GPa
1060 ksi
ISO 527-1/-2
Charpy Impact Unnotched 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Users viewing this material also viewed the following: