Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 75920 cP @Shear Rate 5000 1/s, Temperature 250 °C |
75920 cP @Shear Rate 5000 1/s, Temperature 482 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |