Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 75920 cP

@Shear Rate 5000 1/s,
Temperature 250 °C
75920 cP

@Shear Rate 5000 1/s,
Temperature 482 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)<
Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig..