Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 850000 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
850000 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Novamid® 2320J PA666 Extrusion |
|||
Viscosity | 850000 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
850000 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Novamid® 2420A PA666 Extrusion |
|||
Viscosity | 850000 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
850000 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Novamid® 2420J PA666 Extrusion |