Material Notes:
Extrusion
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
dry; ISO 1183
Moisture Absorption 3.50 %
3.50 %
Sim. To ISO 62
Viscosity 70000 cP

@Shear Rate 10000 1/s,
Temperature 240 °C
70000 cP

@Shear Rate 10000 1/s,
Temperature 464 °F
70000 cP

@Shear Rate 10000 1/s,
Temperature 260 °C
70000 cP

@Shear Rate 10000 1/s,
Temperature 500 °F
70000 cP

@Shear Rate 10000 1/s,
Temperature 280 °C
70000 cP

@Shear Rate 10000 1/s,
Temperature 536 °F
600000 cP

@Shear Rate 0.100 1/s,
Temperature 280 °C
600000 cP

@Shear Rate 0.100 1/s,
Temperature 536 °F
850000 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
850000 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
1.25e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
1.25e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
Viscosity Test 183 cm³/g
183 cm³/g
Viscosity Number; ISO 307, 1157, 1628
Thermal Properties Metric English Comments
Melting Point 193 °C
379 °F
10°C/min,dry; ISO 11357-1/-3