Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 998000 cP @Shear Rate 12.0 1/s, Temperature 285 °C |
998000 cP @Shear Rate 12.0 1/s, Temperature 545 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |