Polymer Property : Kinematic Viscosity = 0.83 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity 0.83 cSt

@Temperature 0.000 °C
0.83 cSt

@Temperature 32.0 °F
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Kinematic Viscosity 0.83 cSt

@Temperature 260 °C
0.83 cSt

@Temperature 500 °F
Duratherm 600 Paraffinic Heat Transfer Fluid
Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to ..
Kinematic Viscosity 0.83 cSt

@Temperature 260 °C
0.83 cSt

@Temperature 500 °F
Duratherm FG Paraffinic Heat Transfer Fluid
Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac..