Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 0.83 cSt @Temperature 0.000 °C |
0.83 cSt @Temperature 32.0 °F |
|
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Kinematic Viscosity | 0.83 cSt @Temperature 260 °C |
0.83 cSt @Temperature 500 °F |
|
Duratherm 600 Paraffinic Heat Transfer Fluid Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to .. |
|||
Kinematic Viscosity | 0.83 cSt @Temperature 260 °C |
0.83 cSt @Temperature 500 °F |
|
Duratherm FG Paraffinic Heat Transfer Fluid Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac.. |