Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.013 cm/cm @Thickness 3.17 mm |
0.013 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 5300 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | Euronil |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm @Time 86400 sec |
0.013 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX MS003 PP LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm @Time 86400 sec |
0.013 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | Euronil |
Nilit Nilamid A3 H ZE High Impact PA66 Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm @Time 86400 sec |
0.013 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WI001 is a compound based on Polybutylene Terephalate resin containing Silicone. Added features include; Inernally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® 42L-N Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® 42LN2-NBK2 Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | |
Toyobo ECOVYLOPET® EMC2301 PET Bottle Recycling Grade, 15% Filler Reinforced Features: PET Bottle Recycling Grade, 15% Filler Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
DSM EcoPaXX® Q-X07208 PA410-I-GF30 % Glass Reinforced, Impact Modified |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
DSM Novamid® 1013GH15 1 NA/BK37 PA6-GF15 15% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® 2S 25 W 20 HL X nat PA610 Product Description: Grilamid 2S 25 W 20 HL X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified and plasticized Polyamide 610, espcailly suitable for extrusion applic.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | Sim. To ISO 294-4 |
DSM Novamid® 3021GH30 NAT PA66-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | Eurotec |
Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | |
Eurotec® Tecomid® NA40 NL RM PA 6.6 low friction and wear Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® L 25 Z PA12-I Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacit.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | Eurotec |
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | |
E-Polymers TEKAMID® JN2 PPE+PA66 Un-reinforced Chemical resistance PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 51 T 20 Polypropylene Homopolymer, 20% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application .. |
|||
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | Sheet |
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs.. |
|||
Linear Mold Shrinkage, Transverse | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ISO DIS 294-4 |
Wellman Wellamid® 42LH-NBK1 General Purpose Nylon 6 Description: General Purpose Nylon 6Information provided by Wellman. |