Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Toyobo ECOVYLOPET® EMC2301 PET Bottle Recycling Grade, 15% Filler Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Toyobo
Trade Name ECOVYLOPET®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo ECOVYLOPET® EMC2301 PET Bottle Recycling Grade, 15% Filler Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: PET Bottle Recycling Grade, 15% Filler Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
Water Absorption 0.060 %
0.060 %
24 hrs at 23°C
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Thickness 2.00 mm
0.012 in/in

@Thickness 0.0787 in
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90
90
Tensile Strength at Break 55.0 MPa
7980 psi
Elongation at Break 1.8 %
1.8 %
Modulus of Elasticity 4.40 GPa
638 ksi
Flexural Strength 100 MPa
14500 psi
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
0.455 MPa
Processing Properties Metric English Comments
Mold Temperature 110 °C
230 °F
Users viewing this material also viewed the following: