Polymer Property : Linear Mold Shrinkage, Transverse = 0.000 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.000 - 0.0160 cm/cm
0.000 - 0.0160 in/in
Average value: 0.00900 cm/cm Grade Count:16
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage, Transverse 0.000 - 0.0300 cm/cm
0.000 - 0.0300 in/in
Average value: 0.0137 cm/cm Grade Count:4
Overview of materials for Polycarbonate-Urethane
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage, Transverse 0.000 - 0.0150 cm/cm
0.000 - 0.0150 in/in
Average value: 0.0102 cm/cm Grade Count:77
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Linear Mold Shrinkage, Transverse 0.000 - 0.0200 cm/cm
0.000 - 0.0200 in/in
Average value: 0.00800 cm/cm Grade Count:7
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
Linear Mold Shrinkage, Transverse 0.000 - 0.0130 cm/cm
0.000 - 0.0130 in/in
Average value: 0.00702 cm/cm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..