Polymer Property : Linear Mold Shrinkage, Transverse = 0.0300 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00160 - 0.0300 cm/cm
0.00160 - 0.0300 in/in
Average value: 0.0152 cm/cm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00170 - 0.0300 cm/cm
0.00170 - 0.0300 in/in
Average value: 0.0116 cm/cm Grade Count:27
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Linear Mold Shrinkage, Transverse 0.000 - 0.0300 cm/cm
0.000 - 0.0300 in/in
Average value: 0.0137 cm/cm Grade Count:4
Overview of materials for Polycarbonate-Urethane
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage, Transverse 0.00900 - 0.0300 cm/cm
0.00900 - 0.0300 in/in
Average value: 0.0164 cm/cm Grade Count:11
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0300 cm/cm
0.0100 - 0.0300 in/in
Average value: 0.0198 cm/cm Grade Count:4
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage, Transverse 0.00600 - 0.0300 cm/cm
0.00600 - 0.0300 in/in
Average value: 0.0143 cm/cm Grade Count:12
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage, Transverse 0.0200 - 0.0300 cm/cm
0.0200 - 0.0300 in/in
Average value: 0.0249 cm/cm Grade Count:3
Overview of materials for Acetal Copolymer, Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0300 cm/cm
0.0100 - 0.0300 in/in
Average value: 0.0189 cm/cm Grade Count:61
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0300 cm/cm
0.00800 - 0.0300 in/in
Average value: 0.0226 cm/cm Grade Count:6
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00960 - 0.0300 cm/cm
0.00960 - 0.0300 in/in
Average value: 0.0162 cm/cm Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0300 cm/cm
0.0100 - 0.0300 in/in
Average value: 0.0141 cm/cm Grade Count:3
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage, Transverse 0.00250 - 0.0300 cm/cm
0.00250 - 0.0300 in/in
Average value: 0.00686 cm/cm Grade Count:60
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Linear Mold Shrinkage, Transverse 0.00110 - 0.0300 cm/cm
0.00110 - 0.0300 in/in
Average value: 0.0132 cm/cm Grade Count:94
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..