Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00040 - 0.00080 cm/cm @Thickness 3.18 mm |
0.00040 - 0.00080 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® SF2-40CF/000 NATURAL Polyphenylene Sulfide (PPS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Transverse | 0.00040 cm/cm | 0.00040 in/in | Post-shrinkage, 150x105x3; 120°C; 4 hour; ISO 2577 |
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.00040 cm/cm | 0.00040 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® B 30 S F30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, flame retardantInformation provided by LANXESS. |