Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00080 - 0.0010 cm/cm

@Time 86400 sec
0.00080 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC
LNP STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 5% PTFE. Added features of this material include: Easy Molding, Electrically Conductive, Wear Resistan..
Linear Mold Shrinkage, Transverse 0.00080 - 0.010 cm/cm

@Time 86400 sec
0.00080 - 0.010 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon EE008E PEI
LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r..