Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00230 - 0.0193 cm/cm | 0.00230 - 0.0193 in/in | Average value: 0.0101 cm/cm Grade Count:33 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |