Polymer Property : Linear Mold Shrinkage, Transverse = 0.0193 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00230 - 0.0193 cm/cm
0.00230 - 0.0193 in/in
Average value: 0.0101 cm/cm Grade Count:33
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..