Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics NORYL WCP700 PPE-TPE
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Linear Mold Shrinkage, Transverse 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Asia Pacific)
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Linear Mold Shrinkage, Transverse 0.0033 cm/cm

@Time 86400 sec
0.0033 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Europe-Africa-Middle East)
Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness.
Linear Mold Shrinkage, Transverse 0.0033 cm/cm
0.0033 in/in
Solvay TECHNYLSTARâ„¢ SX 218 V50 BK 38N-K PA6, 50% glass filled, DRY
Description: High stiffness materials Technylstar polyamide 6, reinforced with 50% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: ..
Linear Mold Shrinkage, Transverse 0.0033 cm/cm
0.0033 in/in
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY
Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i..
Linear Mold Shrinkage, Transverse 0.0033 cm/cm
0.0033 in/in
ISO 294-4
Solvay Specialty Polymers Kalix® 2955 Polyamide, High Performance (HPPA), Glass Fiber
Kalix® 2955 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is specifically formulated for high strength and stiffness applications where ..
Linear Mold Shrinkage, Transverse 0.0033 cm/cm
0.0033 in/in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific)
LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006.
Linear Mold Shrinkage, Transverse 0.0033 cm/cm
0.0033 in/in
GB/T 15585-1995
Sichuan Deyang Haton® hGR515 Polyphenylene Sulfide/PA Alloy
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
Linear Mold Shrinkage, Transverse 0.0033 cm/cm
0.0033 in/in
ISO 294-4
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY
Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go..
Copyright © lookpolymers.com All Rights Reserved