Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00620 - 0.0210 cm/cm
0.00620 - 0.0210 in/in
Average value: 0.0156 cm/cm Grade Count:8
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..