Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00100 - 0.0210 cm/cm
0.00100 - 0.0210 in/in
Average value: 0.00968 cm/cm Grade Count:124
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0210 cm/cm
0.0100 - 0.0210 in/in
Average value: 0.0144 cm/cm Grade Count:14
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Linear Mold Shrinkage, Transverse 0.00900 - 0.0210 cm/cm
0.00900 - 0.0210 in/in
Average value: 0.0153 cm/cm Grade Count:8
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Linear Mold Shrinkage, Transverse 0.00930 - 0.0210 cm/cm
0.00930 - 0.0210 in/in
Average value: 0.0140 cm/cm Grade Count:5
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Linear Mold Shrinkage, Transverse 0.00620 - 0.0210 cm/cm
0.00620 - 0.0210 in/in
Average value: 0.0156 cm/cm Grade Count:8
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..