Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00630 - 0.0170 cm/cm
0.00630 - 0.0170 in/in
Average value: 0.0114 cm/cm Grade Count:21
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..