Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00250 - 0.0170 cm/cm
0.00250 - 0.0170 in/in
Average value: 0.00629 cm/cm Grade Count:25
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Linear Mold Shrinkage, Transverse 0.00630 - 0.0170 cm/cm
0.00630 - 0.0170 in/in
Average value: 0.0114 cm/cm Grade Count:21
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage, Transverse 0.00700 - 0.0170 cm/cm
0.00700 - 0.0170 in/in
Average value: 0.0106 cm/cm Grade Count:22
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage, Transverse 0.00900 - 0.0170 cm/cm
0.00900 - 0.0170 in/in
Average value: 0.0117 cm/cm Grade Count:4
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Linear Mold Shrinkage, Transverse 0.000900 - 0.0170 cm/cm
0.000900 - 0.0170 in/in
Average value: 0.00846 cm/cm Grade Count:200
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..
Linear Mold Shrinkage, Transverse 0.000800 - 0.0170 cm/cm
0.000800 - 0.0170 in/in
Average value: 0.00534 cm/cm Grade Count:241
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Linear Mold Shrinkage, Transverse 0.00460 - 0.0170 cm/cm
0.00460 - 0.0170 in/in
Average value: 0.0117 cm/cm Grade Count:29
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0170 cm/cm
0.00500 - 0.0170 in/in
Average value: 0.0113 cm/cm Grade Count:11
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..