Polymer Property : Linear Mold Shrinkage, Transverse = 0.0086 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0086 cm/cm

@Thickness 0.750 - 2.30 mm
0.0086 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized
Linear Mold Shrinkage, Transverse 0.0086 cm/cm
0.0086 in/in
ISO 2577, 294-4
BASF Ultrason® E 2010 MR SW 10111 PESU
Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF
Linear Mold Shrinkage, Transverse 0.0086 cm/cm
0.0086 in/in
ISO 294
BASF Ultrason E 2010 PES
Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Linear Mold Shrinkage, Transverse 0.0086 cm/cm
0.0086 in/in
ISO 2577, 294-4
BASF Ultrason® E 2010 HC PESU
Information provided by BASF
Linear Mold Shrinkage, Transverse 0.0086 cm/cm
0.0086 in/in
ISO 2577, 294-4