Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0104 cm/cm | 0.0104 in/in | |
Plastcom SLOVAMID 6/66 CF 30 PA6/66, 30% carbon fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 30% of carbon fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-.. |
|||
Linear Mold Shrinkage, Transverse | 0.0104 cm/cm | 0.0104 in/in | |
Plastcom SLOVASTER® B GB 30 PBT, 30% glass beads FeaturesPBT for injection moulding, chemically reinforced with 30% glass beads. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Linear Mold Shrinkage, Transverse | 0.0104 cm/cm | 0.0104 in/in | 150x105x3, 260°C / MT 80°C; 500 bar; ISO 2577 |
Lanxess Pocan® KU 2-7241 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, flame retardant, improved impact strengthInformation provided by LANXESS. |