Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0108 cm/cm
0.0108 in/in
Plastcom SLOVASTER® B/A GF 20 PBT, 20% glass fibre
FeaturesPBT/ASA for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben..
Linear Mold Shrinkage, Transverse 0.0108 cm/cm
0.0108 in/in
Solvay TECHNYLSTARâ„¢ S 218 MZ20 V10 Black 2N PA6, 20% mineral, 10% glass filled, DRY
Description: TECHNYL STAR Polyamide, 20% mineral filled and 10% of glass fiber reinforced, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe a..
Linear Mold Shrinkage, Transverse 0.0108 cm/cm

@Time 86400 sec
0.0108 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific)
This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region.