Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.010 - 0.0125 cm/cm

@Thickness 3.17 mm
0.010 - 0.0125 in/in

@Thickness 0.125 in
Ovation Polymers Opnyl OP66GF13 Nylon 66, 13% Glass Reinforced
Nylon 66 - Glass reinforced (13 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared..
Linear Mold Shrinkage, Transverse 0.010 - 0.0125 cm/cm
0.010 - 0.0125 in/in
LATI Latamid 6 S/30 PA 6, 30% Glass Bead Reinforced
Polyamide 6 (PA6) based compound. Glass beads. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Linear Mold Shrinkage, Transverse 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Linear Mold Shrinkage, Transverse 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
LATI Later 4 G/30-V0HF1 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe..
Linear Mold Shrinkage, Transverse 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
LATI Laticonther 52/35 CP1/45 PP Homopolymer
High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Linear Mold Shrinkage, Transverse 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
LATI Latilub 66-01M G/15 PA66, 15% Glass Fiber Reinforced, Molybdenum disulphide Filled
Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Linear Mold Shrinkage, Transverse 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
LATI Latilub 66-20T G/20 PA66, 20% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..
Linear Mold Shrinkage, Transverse 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
LATI Latishield 66-10A G/15 PA66, Steel/Glass Fiber Reinforced
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Linear Mold Shrinkage, Transverse 0.010 - 0.0125 cm/cm
0.010 - 0.0125 in/in
LATI Latishield 66-13A G/30 PA66, Steel/Glass Fiber Reinforced
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Linear Mold Shrinkage, Transverse 0.0085 - 0.0125 cm/cm
0.0085 - 0.0125 in/in
ISO DIS 294-4
Wellman Wellamid® GF33-66 XE-NBK1 33% Glass Fiber Reinforced, Engineering Grade Nylon 66
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.00650 - 0.0125 cm/cm
0.00650 - 0.0125 in/in
Average value: 0.0101 cm/cm Grade Count:4
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage, Transverse 0.0085 - 0.0125 cm/cm
0.0085 - 0.0125 in/in
LATI Latilub 88/10-10T Y/10 PEEK, 10% Aramid Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..