Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |
Plastcom SLOVALEN PQ 81 T 30 PP, 30% mineral filling FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 30 FRA 5 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 35 FRI 3 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-h.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | 60x60x2; 280°C / MT 80°C; 600 bar; ISO 2577 |
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibersInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | 150x105x3; 280°C / MT 80°C; 400 bar; ISO 2577 |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | 150x105x3; 280°C / MT 80°C; 400 bar; ISO 2577 |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm @Thickness 3.00 mm |
0.0085 in/in @Thickness 0.118 in |
Mold Temp 80°C; Melt Temp 280°C; 400 bar; ISO 294-4 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.0115 cm/cm | 0.0085 - 0.0115 in/in | |
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.0105 cm/cm | 0.0085 - 0.0105 in/in | |
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.010 cm/cm | 0.0085 - 0.010 in/in | |
LATI Lapex R G/10 PPSU, 10% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.0115 cm/cm | 0.0085 - 0.0115 in/in | |
LATI Latamid 66 H2 G/25 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.0115 cm/cm | 0.0085 - 0.0115 in/in | |
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.0115 cm/cm | 0.0085 - 0.0115 in/in | |
LATI Latiohm 66-05 PD01 G/20 PA66, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.0105 cm/cm | 0.0085 - 0.0105 in/in | |
LATI Latistat 52/7-02 MI/30 PP Homopolymer, 30% Mica Filled Dissipative product based on Polypropylene homopolymer (PPh). Mica filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |
Solvay TECHNYL® A 218 V25 Black 21NHFE PA66, 25% glass fiber, DRY Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |
Solvay TECHNYL® A 218 V25 NAT BA PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: Asia PacificProduct Application.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |
Solvay TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: EuropeProduct Applications: Thi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | ISO 294-4 |
Solvay Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This p.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |
Solvay TECHNYL® C 52G1 V25 Grey R7035 (XC 1329/A) PA6, DRY Description: Polyamide 6, Glass-filled, glow-wire modified, color stabilized, lubricated for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Application.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.0125 cm/cm | 0.0085 - 0.0125 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF33-66 XE-NBK1 33% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.0105 cm/cm | 0.0085 - 0.0105 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT1525-BK 15% Glass Fiber Reinforced, Impact Modified Nylon 6 Description: Glass Fiber Reinforced, Impact Modified Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.0105 cm/cm | 0.0085 - 0.0105 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFT15N050-WBK 15% Glass Fiber Reinforced, Toughened, Weatherable Nylon 66 Description: Glass Fiber Reinforced, Toughened, Weatherable Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |
Toyobo TS501 PPS, 50% Glass Fiber Reinforced Key Feature: High stiffnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent physical, e.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm @Thickness 2.00 mm |
0.0085 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | ISO 2577 |
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry) Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.Information provided by BASF |
|||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | ISO 2577, 294-4 |
BASF Ultrason® E 2010 MR HP PESU Description: Unreinforced, medium viscosity standard injection molding grade for improved demolding behavior with Mold Release. PES-Blend with improved processibility. (High Productivity) Abbreviate.. |
|||
Linear Mold Shrinkage, Transverse | 0.0085 - 0.0125 cm/cm | 0.0085 - 0.0125 in/in | |
LATI Latilub 88/10-10T Y/10 PEEK, 10% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |