Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0233 cm/cm
0.0233 in/in
STN 64 0808
Plastcom SLOVALEN PC 78 FRD 3 Polypropylene Copolymer, Halogen Flame Retardant
FeaturesDetermined for environment where contact with water is possible because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machine..
Linear Mold Shrinkage, Transverse 0.0233 cm/cm
0.0233 in/in
Solvay TECHNYL® eXten D 437P PA6.10
Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia..