Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0392 cm/cm @Thickness 3.17 mm |
0.0392 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 3300 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |