Polymer Property : Linear Mold Shrinkage = 0.013 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0080 - 0.013 cm/cm

@Thickness 1.00 - 2.50 mm
0.0080 - 0.013 in/in

@Thickness 0.0394 - 0.0984 in
ASTM D955
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage 0.0070 - 0.013 cm/cm

@Thickness 1.60 mm
0.0070 - 0.013 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 4140-201D 40% Glass Fiber Filled
Product Description: A glass fiber 40% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.0070 - 0.013 cm/cm

@Thickness 1.60 mm
0.0070 - 0.013 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax CCP ABS/PBT 7320H-104 20% Glass Fiber Filled
Product Description: A 20% glass fiber reinforced injection molding grade. Characteristics:Low warp age and excellent dimensionally stable Excellent electrical property Excellent mechanic and chemi..
Linear Mold Shrinkage 0.010 - 0.013 cm/cm

@Thickness 3.00 mm
0.010 - 0.013 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-402FR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0080 - 0.013 cm/cm

@Thickness 3.00 mm
0.0080 - 0.013 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.010 - 0.013 cm/cm

@Thickness 3.00 mm
0.010 - 0.013 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0080 - 0.013 cm/cm

@Thickness 3.00 mm
0.0080 - 0.013 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-779 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..