Linear Mold Shrinkage 0.018 - 0.022 cm/cm

@Thickness 6.35 mm
0.018 - 0.022 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.018 - 0.022 cm/cm

@Thickness 6.35 mm
0.018 - 0.022 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.015 - 0.022 cm/cm

@Thickness 3.00 mm
0.015 - 0.022 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.015 - 0.022 cm/cm

@Thickness 3.00 mm
0.015 - 0.022 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.015 - 0.022 cm/cm

@Thickness 3.00 mm
0.015 - 0.022 in/in

@Thickness 0.118 in
DAM
Toyobo T-661 Nylon 66, Standard Grade (Conditioned)
Features: Non-reinforced, Standard GradeInformation provided by Toyobo.
Linear Mold Shrinkage 0.015 - 0.022 cm/cm

@Thickness 3.00 mm
0.015 - 0.022 in/in

@Thickness 0.118 in
Toyobo T-661 Nylon 66, Standard Grade (DAM)
Features: Non-reinforced, Standard GradeInformation provided by Toyobo.