Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.018 cm/cm @Thickness 3.20 mm |
0.018 in/in @Thickness 0.126 in |
Parallel; DAM; ASTM D955 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm @Thickness 3.17 mm |
0.018 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm @Thickness 6.35 mm |
0.018 - 0.022 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm @Thickness 6.35 mm |
0.018 - 0.022 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.018 - 0.023 cm/cm @Thickness 3.00 mm |
0.018 - 0.023 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-222SA Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm @Thickness 3.20 mm |
0.018 - 0.021 in/in @Thickness 0.126 in |
Flow, 24h; ASTM D955 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |