Physical Properties Metric English Comments
Melt Index of Compound 0.35 g/10 min
0.35 g/10 min
Condition 190/2.16; ASTM D1238
Chevron Phillips Marlex® HHM 5202LD HDPE Blow Molding Resin  (discontinued **)
Resin Type: Hexene CopolymerCharacteristics: Good stiffnessExceptional processabilityGood ESCRApplications: Household & industrial chemical containersInformation provided by Chevron Phillips.
Melt Index of Compound 0.35 g/10 min
0.35 g/10 min
Condition 190/2.16; ASTM D1238
Chevron Phillips Marlex® 7104 LLDPE Sheet Extrusion
Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRGood melt strengthExcellent flexibilityGood processabilityGood glossHigh COFApplications: Landfill coversFlat and round-die productsCoext..
Melt Index of Compound 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Amco PRIMATOP HDPE 004955HP Blow Molding Polyethylene
HDPE 003955PZ features zinc stearate additive and is used for injection blow molding.Former A-Top Polymers product; part of Amco product line since 2013.
Melt Index of Compound 0.35 g/10 min
0.35 g/10 min
ASTM D1238
Amco PRIMATOP HDPE 003952 Phillips Process Hexene Copolymer
HDPE 003952 features excellent stiffness and stress crack resistance properties. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part of Amco produ..
Melt Index of Compound 0.35 g/10 min
0.35 g/10 min
ASTM D1238
Amco PRIMATOP HDPE 003955BAS Hexene Copolymer
HDPE 003955BAS features excellent stiffness, stress crack resistance properties, and antistat. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part..
Melt Index of Compound 0.35 g/10 min
0.35 g/10 min
ASTM D1238
Amco PRIMATOP HDPE 003955P Phillips Process Hexene Copolymer
HDPE 003955P features excellent stiffness and stress crack resistance properties. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part of Amco prod..
Melt Index of Compound 0.35 g/10 min
0.35 g/10 min
ASTM D1238
Amco PRIMATOP HDPE 003955PZ Phillips Process Hexene Copolymer
HDPE 003955P features excellent stiffness and stress crack resistance properties. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part of Amco prod..
Melt Index of Compound 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Chevron Phillips Marlex® HHM 5502LW Polyethylene; HDPE
High density polyethylene. This high molecular weight, hexene copolymer with synthetic antistatic agent is tailored for lightweight blow molded containers that: Require excellent stiffnessRequire ..