Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.45 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow 500.00 Developmental Performance Polypropylene Polymer D 500.00 Developmental Performance Polymer is a performance plastic designed for cut sheet thermoforming. The propylene-based polymer offers improved formability in large part thermoforming applica.. |
|||
Melt Index of Compound | 0.45 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ DFDA-1098 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1098 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization .. |
|||
Melt Index of Compound | 0.45 g/10 min | 0.45 g/10 min | ASTM D1238 |
Amco PRIMATOP PP CO 005NB Fractional Melt Polypropylene Copolymer Features:heat aging resistanceimpact resistancelow temperature melt strengthgood stiffnessApplications:containerspipestoysextrusion coatingFormer A-Top Polymers product; part of Amco product line si.. |