Amco PRIMATOP PP CO 005NB Fractional Melt Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Amco Plastic Materials
Trade Name PRIMATOP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco PRIMATOP PP CO 005NB Fractional Melt Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:heat aging resistanceimpact resistancelow temperature melt strengthgood stiffnessApplications:containerspipestoysextrusion coatingFormer A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Specific Gravity 0.902 g/cc
0.902 g/cc
method B; ASTM D792
Melt Index of Compound 0.45 g/10 min
0.45 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 27.6 MPa
4000 psi
50 mm/min; ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
.05 in/min, 1% Secant; ASTM D790
Izod Impact, Notched NB

@Temperature 22.8 °C
NB

@Temperature 73.0 °F
Method A; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
190 °F
ASTM D648