Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut.. |
|||
Melt Index of Compound | 1.6 g/10 min @Temperature 190 °C |
1.6 g/10 min @Temperature 374 °F |
ASTM D1238 |
Mitsui ADMER® AT2018A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8440 Polyolefin Elastomer Description: Engage® 8440 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It is an excellent thermoplastic elastomer .. |