Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 230 °C |
22 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs S00 ABS, High Flow Information provided by Polykemi AB |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 230 °C |
22 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs S00 AS UV ABS, High Flow, UV-Stabilized, Antistatic Information provided by Polykemi AB |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 230 °C |
22 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs S20 ABS Information provided by Polykemi AB |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific) Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi.. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Melt Index of Compound | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BFL4000U PC (Asia Pacific) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Melt Index of Compound | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 260 °C |
22 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Melt Index of Compound | 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
22 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BFL4000U PC Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Melt Index of Compound | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5049 400 Micron LDPE Powder Description: ICOFLO 510-5049 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5050 500 Micron LDPE Powder Description: ICOFLO 510-5050 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5051 800 Micron LDPE Powder Description: ICOFLO 510-5051 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOTEXâ„¢ 520-5016 300 Micron LDPE Powder Description: ICOTEX 520-5016 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Melt Index of Compound | 22 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fa.. |
|||
Melt Index of Compound | 22 g/10 min | 22 g/10 min | ASTM D1238 |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 300 °C |
22 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific) DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 250 °C |
22 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX1007 PPE+PS Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 360 °C |
22 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 9076 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 280 °C |
22 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W.. |
|||
Melt Index of Compound | 22 g/10 min @Temperature 230 °C |
22 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ P50DFR Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Melt Index of Compound | 22 g/10 min @Temperature 230 °C |
22 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ P55B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Melt Index of Compound | 22 g/10 min @Temperature 230 °C |
22 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ P55U Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |
|||
Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 372 °C |
22 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ FEP 6322Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6322Z was designed primarily for high-speed extrusion for wire insulation. Its distinguishing features include:High extrusion speedHigh thermal stabilityWide processing windowSuperior ele.. |
|||
Melt Index of Compound | 22 - 29 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 - 29 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 28-25 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-25 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melt Index of Compound | 22 - 29 g/10 min @Load 2.16 kg, Temperature 190 °C |
22 - 29 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 33-25 Copolymer Ethylene - Vinyl Acetate EVATANE® 33-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-25 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melt Index of Compound | 22 g/10 min @Load 1.20 kg, Temperature 224 °C |
22 g/10 min @Load 2.65 lb, Temperature 435 °F |
ASTM D1238 |
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat.. |
|||
Melt Index of Compound | 22 g/10 min @Temperature 230 °C |
22 g/10 min @Temperature 446 °F |
ASTM D1238 |
Amco PRIMATOP PP CO 220-23 Impact Polypropylene Copolymer PP CO 220-23 has easy mold flow and excellent dimensional stability. Applications include closures, housewares, and small appliance applications.Former A-Top Polymers product; part of Amco product l.. |