ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Masterbatch Grade
Manufacturer ICO Polymers (A Schulman Inc.)
Trade Name ICOTEX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fast and accurate melting. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.914 g/cc
0.0330 lb/in³
ASTM D1505
Particle Size >= 150 µm
>= 150 µm
pan, 10%
<= 500 µm
<= 500 µm
sieve < 5%
Melt Index of Compound 22 g/10 min

@Load 2.16 kg,
Temperature 190 °C
22 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.00 MPa
1310 psi
ASTM D638
Tensile Strength, Yield 9.00 MPa
1310 psi
50 mm/min; ASTM D638
Elongation at Break 90 %
90 %
50 mm/min; ASTM D638
Thermal Properties Metric English Comments
Melting Point 100 °C
212 °F
DSC; ASTM D3418
140 °C
284 °F
fusing temperature
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D638
Descriptive Properties Value Comments
Max Dry Flow max 31 sec/100g
ASTM