Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 47 g/10 min @Load 5.00 kg, Temperature 300 °C |
47 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP STAT-KON DX09303C PC (Asia Pacific) LNP* Stat-Kon* DX09303C is carbon fiber filled polycarbonate composite with high modulus, good flow ability, and high level of cleanliness for the most demanding application. A unique feature of thi.. |