Material Notes:
LNP* Stat-Kon* DX09303C is carbon fiber filled polycarbonate composite with high modulus, good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is its low C18-C40 hydrocarbons. This compound is manufactured using LNP CCS Technology.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0010 - 0.0025 cm/cm

@Thickness 3.20 mm
0.0010 - 0.0025 in/in

@Thickness 0.126 in
SABIC Method
Melt Index of Compound 47 g/10 min

@Load 5.00 kg,
Temperature 300 °C
47 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 161 MPa
23400 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 20.13 GPa
2920 ksi
5 mm/min; ASTM D638
Flexural Strength 246 MPa
35700 psi
ASTM D790
Flexural Modulus 18.0 GPa
2610 ksi
ASTM D790
Izod Impact, Notched 0.820 J/cm
1.54 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.01 J/cm
11.3 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 4.40 µm/m-°C

@Temperature -40.0 - 40.0 °C
2.44 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 59.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 125 °C

@Thickness 3.20 mm
257 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 5000 - 500000 ohm
5000 - 500000 ohm
ASTM D257