Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 52 g/10 min @Load 2.16 kg, Temperature 265 °C |
52 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developed for automotive bezel application that requires basecoat + .. |
|||
Melt Index of Compound | 52 g/10 min @Load 2.16 kg, Temperature 265 °C |
52 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Melt Index of Compound | 52 g/10 min @Load 5.00 kg, Temperature 280 °C |
52 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PVX0901 PPE+PS (Asia Pacific) Multi purpose V1 grade |
|||
Melt Index of Compound | 52 g/10 min | 52 g/10 min | ASTM D1238, modified |
DuPont Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin Elvax® 40W has a higher vinyl acetate content compared with the other Elvax® resins resulting in higher elongation, reduced hardness, improved solubility and adhesion, and significant differences .. |
|||
Melt Index of Compound | 52 g/10 min @Load 8.70 kg, Temperature 190 °C |
52 g/10 min @Load 19.2 lb, Temperature 374 °F |
ASTM D1238 |
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l.. |