Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.00e+6 cP @Shear Rate 270 1/s, Temperature 230 °C |
1.00e+6 cP @Shear Rate 270 1/s, Temperature 446 °F |
|
Noltex Soarnol® BS3803 Ethylene Vinyl Alcohol Copolymer Modified ET3803; New Stretchable EVOH. Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows .. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 190 1/s, Temperature 230 °C |
1.00e+6 cP @Shear Rate 190 1/s, Temperature 446 °F |
|
Noltex Soarnol® ET3803 Ethylene Vinyl Alcohol Copolymer Medium ethylene content. Suitable for packaging a wet product in a wet environment. Preferred for use in forming webs for meat and cheese packaging. Ethylene content 38 mol%. Volatile matter 0.3%... |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 - 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 - 716 °F |
Average value: 5.50e+6 cP Grade Count:5 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Viscosity | 1.00e+6 cP | 1.00e+6 cP | Melt |
3M Dyneon™ TF 9207 PTFE
(discontinued **) Low molecular weight virgin PTFEAgglomerate particlesEasily deagglomeratedInformation provided by Dyneon, A 3M Company |
|||
Viscosity | 1.00e+6 cP | 1.00e+6 cP | Gum Viscosity |
Shin-Etsu Silicones KF-9003 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 1.00e+6 cP | 1.00e+6 cP | Gum Viscosity |
Shin-Etsu Silicones KF-9012 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 1.00e+6 cP | 1.00e+6 cP | Gum Viscosity |
Shin-Etsu Silicones KF-9004 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 1.00e+6 cP | 1.00e+6 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KE2001-50A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | >= 1.00e+6 cP | >= 1.00e+6 cP | Part A |
Master Bond EP42HT-2ND-2Med Heat Resistant, Medical Grade Non-Drip Epoxy Master Bond Polymer System EP42HT-2ND2MED (Black) is a room temperature curable two component epoxy adhesive and sealant featuring high temperature resistance along with outstanding chemical resista.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F132 PA6 Film Extrusion, High Viscosity |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F132-C1 PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F132-E1 PA6 Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F132-E2 PA6 High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F234-C PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 1.00e+6 cP @Temperature 160 °C |
1.00e+6 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1616E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EA-LR43 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® XP32-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-201 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-210 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided .. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 cP | 1.00e+6 cP | Melt Velocity |
Asahi Glass Fluon® ETFE A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Appeel® LSR 1181 Modified EVA Lidding Sealing Resin Appeel® 1181 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
|
DuPont Bynel® 3933 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |